Composite biodegradable materials based on polyhydroxyalkanoate

Gogotov, I.N.; Gerasin, V.A.; Kniazev, I.V.; Antipov, E.M.; Barazov, S.K.

Prikladnaia Biokhimiia i Mikrobiologiia 46(6): 659-665

2010


ISSN/ISBN: 0555-1099
PMID: 21261076
Document Number: 639379
Conditions for the processing and mixing of biodegradable polymers at temperatures less than their thermal destruction (130-150 degrees C) using standard equipment have been identified. The structure of the polyhydroxybutyrate/valerate (PHB/V) copolymer has been revealed and peculiarities of the crystal phase formation at different monomer ratios have been investigated. It was shown that pure PHB with molecular mass 180-270 kDa has elastic module approximately 1.2 GPa, strength approximately 25 MPa, and elongation at break approximately 10%. The most active biodestructors of PHB, PHB/V, and their composites have been selected (Aspergillus caespitosus), and the ability of basidiomycete Panus tigrinus to biodegrade polyalkanoates was demonstrated for the first time. It was shown that A. caespitosus degraded PHB/V and Biopol films along with the PHB with the destruction rate depending on the technology of the film production, on the molecular mass, and on the extend of the polymer crystallinity.

Document emailed within 1 workday
Secure & encrypted payments