An improved deresining method for semithin sections embedded-epoxy resin

Jiang, H.Y.; Shen, M.; Feng, D.Y.

Hunan Yi Ke da Xue Xue Bao 25(1): 85-86

2000


ISSN/ISBN: 1000-5625
PMID: 12212262
Document Number: 521133
Deresining must be performed for HE, specific histochemical staining and immunohistochemical detection on semithin-sections embedded-epoxy resin. The deresining process in general methods had to take 24 hours, and the semithin-sections were easily separated from slides. An improved method was introduced in this paper, by which deresining time was only 5 minutes, and it could also avoid the separation of semithin-sections from the slides. The staining result was very good, and the resolving power of images was high.