Etched-porcelain resin-bonded full-veneer crowns: in vitro fracture resistance

Jensen, M.E.; Sheth, J.J.; Tolliver, D.

Compendium 10(6): 336-8 340-1 344-7

1989


ISSN/ISBN: 0894-1009
PMID: 2605607
Document Number: 337751
A recent study showed that both anterior and posterior glass ionomer-bonded crowns were significantly weaker than natural teeth. However, the fracture resistance of resin-bonded anterior crowns exceeded the strength of their size-matched controls. The three cement types were significantly different, with the average strength for Gluma, a-bonded crowns being the highest, then the Scotch-bond, b-bonded crowns, while Ketac Bond, c glass ionomer cemented crowns were the weakest. This pilot study indicates that the resin-bonded etched-porcelain full-veneer crowns are almost as strong as natural teeth and significantly stronger than glass ionomer-bonded crowns.