Methods for the preparation of ceramic jacket crowns by means of channel grinders
Gumezki, R.A.
Stomatologie der DDR 27(10): 669-671
1977
ISSN/ISBN: 0302-4725 PMID: 270854 Document Number: 111583
Self-designed grooving grinders are used for the controlled reduction of dental hard tissues (fig. 1-4). Thereby the preparation of the smooth surfaces and shoulder becomes more accurate and less time-consuming. This method has been used on 59 teeth without complications.
Document emailed within 1 workday
Related Documents
Von Majewsky, I. 1981: Plaque retention by plastic jacket crowns and ceramic jacket crowns Stomatologie der DDR 31(8): 578-582Moll, A. 1971: Modified impression of root stumps for the manufacture of cast pivot crowns, respectively nuclear build-up of jacket crowns by means of rubberelastic impression materials Zwr 80(2): 51-52
Gonzalez, J.S. 1989: Preparation of Dicor glass-ceramic crowns Zwr 98(4): 371
Perelmuter, S.; Liger, F. 1988: Ceramic crowns and bridges without metallic support: effect on preparation L' Information Dentaire 70(33): 3063-3070
Vadachkoria, D.; Vadachkoria, O. 2017: Clinical Protocols: Preparation, Impression and Bonding of All-Ceramic Glass-Based Disilicate Lithium Crowns: Review and Case Report Georgian Medical News 2017(265): 94-98
Anusavice, K.J. 1997: Reducing the failure potential of ceramic-based restorations. Part 2: Ceramic inlays, crowns, veneers, and bridges General Dentistry 45(1): 30-35
Chai, J.; Takahashi, Y.; Sulaiman, F.; Chong, K.; Lautenschlager, E.P. 2000: Probability of fracture of all-ceramic crowns International Journal of Prosthodontics 13(5): 420-424
Yoshinari, M.; Dérand, T. 1994: Fracture strength of all-ceramic crowns International Journal of Prosthodontics 7(4): 329-338
Biffar, R.; Weltzsch, U. 1989: Accuracy of fit of veneer crowns with ceramic shoulders Deutsche Zahnarztliche Zeitschrift 44(10): 779-782
Xu, M.; Yang, F.; Wang, R.-f. 2012: Evaluation of marginal adaptation of three different copings of metal-ceramic crowns Shanghai Kou Qiang Yi Xue 21(2): 154-156
Zhang, B.; Zhao, Y.; Wang, H. 2000: Three-dimensional finite element analysis of all-ceramic crowns of the posterior teeth Hua Xi Yi Ke da Xue Xue Bao 31(2): 147-8 164
Lin, X.; Xu, Y.; Yang, Q.; Zhang, D. 2017: Research on the mechanical differences of machinable lithium disilicate all-ceramic crowns Sheng Wu Yi Xue Gong Cheng Xue Za Zhi 34(1): 48-52
McLaren, E.A.; Terry, D.A. 2002: CAD/CAM systems, materials, and clinical guidelines for all-ceramic crowns and fixed partial dentures Compendium of Continuing Education in Dentistry 23(7): 637
Passos, L.; Torrealba, Y.; Linke, B.; Street, A.; Passos, S. 2018: Fracture strength of CAD/CAM posterior ceramic crowns after manual enhancement of occlusal morphology International Journal of Computerized Dentistry 21(3): 191-200
Zhong, Q.; Peng, Y.; Wu, X.-Y.; Weng, J.-W. 2016: Effects of repeated firing on microleakage of selective laser melting ceramic crowns Shanghai Kou Qiang Yi Xue 25(6): 663-667
Ge, J.; Wang, X-zhi.; Feng, H-lan. 2006: Influence of different post core materials on the color of Empress 2 full ceramic crowns Chinese Medical Journal 119(20): 1715-1720
Nakamura, Y.; Anusavice, K.J. 1998: Marginal distortion of thermally incompatible metal ceramic crowns with overextended margins International Journal of Prosthodontics 11(4): 325-332
Liu, Y.-h.; Han, K.; Liu, L.; Xu, C.-d. 2003: The influences of shoulder porcelain length on the stress distribution of metal-ceramic crowns Zhonghua Kou Qiang Yi Xue Za Zhi 38(2): 119-122
Hartung, F.; Kordass, B. 2006: Comparison of the contact surface pattern between virtual and milled Cerec 3D full-ceramic crowns International Journal of Computerized Dentistry 9(2): 129-136
Jun, S.K.; Oh, J.S. 2005: Achieving anterior aesthetics in the geriatric patient using full-coverage metal-ceramic crowns Practical Procedures and Aesthetic Dentistry: Ppad 17(1): 57-59